Kraiburg THERMOLAST K® CO/VC Series TP6MCZ Black TPE
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
- Adhesion to technical thermoplastics with improved compression set
- Adhesion to ABS, SAN,ASA, PC, PC/ABS, PC/PBT
- For patent free comolded parts
- Good flow characteristics
- Excellent adhesion even with soft compounds
- Improved compression set
- UL94 HB listed compounds available
Typical Applications: - Electric and electronic components
- Seals
- Functional elements
- Hard/soft applications with higher requirement to compression set (e.g. indicator, PC-lens encapsulation, additional break light)
- Coextrusion: sealing
Material Advantages: - Excellent adhesion without pretreatment
- Excellent compression set
- Adhesion even under difficult conditions
- Easy to color
- Tactile surface (soft touch)
- Good flow characteristics
- Low emission (fogging)
Processing: - Low back pressure
- High injection speed and pressure
- Easy demolding
- Extrusion also possible
Information provided by Kraiburg TPE.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Flammability, UL94
- Processing Temperature
- Drying Temperature
- Dry Time
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|