Kraiburg THERMOLAST K® HQ/EC Series TP8CCZ Black Cable Extrusion TPE
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
- Black compound for cable extrusion
- Substitute for PVC-P
- Extremely flexible material
- Flexible in low temperatures
- Outdoor use
Typical Applications: - Transmission cables
- Loudspeaker cables
- Connecting cables
Material Advantages: - PVC free
- Adhesion to polyolefins
- Excellent electric insulation
- High elasticity
- Smooth surface
- Weathering resistant
Processing: - Standard extruders (e.g. universal or polyolefin extruder are recommended)
- Breaker plate and screen pack are recommended
Information provided by Kraiburg TPE.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Color
- Compression Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|