Kraiburg THERMOLAST K® HT Series TC4HTT Transparent TPE, Outdoor Grade
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
- Transparent compounds with ideal UV resistance for outdoor applications
- Substitute of silicone rubber or PVC
- Nice design possibilities by coloring the compounds with a suitable polyolefin masterbatch
Typical Applications: - Outdoor sports/Outdoor games::
- Water sports (e.g. flippers, snorkel, diving goggles, etc.)
- Skiing (e.g. binding plates and etc.)
Material Advantages: - UV resistant (passed 450 hour sun test without yellowing)
- Transparent
- High elasticity
- Particularly for parts with large thickness
- East to color
- Adhesion to polyolefins
- 100% recyclable
- Very good flow characteristics
Processing: - Like polyolefins
- For ideal transparency a cool mold is recommended
- Apply back pressure for parts with thick wall
Information provided by Kraiburg TPE.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Color
- Gate
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|