Kraiburg THERMOLAST K® HT/E Series TC4CHT Transparent Extrusion TPE
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
- Transparent compound for extrusion
- Substitute for silicon and PVC-P
- Extremely flexible material
- Coloring in any shade
Typical Applications: - Design (e.g. grip elements and functional elements for furniture)
- Seals
- Profiles (e.g. side wall protection)
Material Advantages: - Smooth surface
- High elasticity
- Adhesion to polyolefins
Processing: - Standard extruders (e.g. universal or polyolefin extruder are recommended)
- Breaker plate and screen pack are also recommended
- Also suitable for injection molding
Information provided by Kraiburg TPE.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Color
- Compression Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|