Kraiburg THERMOLAST K® IC/U Series TP6HKZ Exterior Automotive Sealing TPE
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
- Black compound for exterior automotive sealing applications
- Excellent sealing performance
Typical Applications: - Headlamp seals
- Air drag sealing
Material Advantages: - Good compression set
- High resistance to UV-light exposure and weathering
- Meets Florida-/Kalahari test and VW PV 3930, 3929
- Adhesion to PP
Processing: - Like polyolefins
- High injection speed and pressure
- No predrying
- Easy demolding
Information provided by Kraiburg TPE.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
- Processing Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|