Kuraray SEPTON® A2, Hot Melt Adhesive

 

Subcategory: Elastomer, TPE; Adhesive; Thermoplastic

Material Notes:
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block copolymers, which exhibit rubber-like properties over a wide range of temperatures. SEPTON®'s remarkable characteristics include:

  • Excellent Mechanical Properties
  • Good Weatherability
  • Excellent Low Temperature Properties
  • Excellent Electrical Properties
  • Superior Heat Resistance
  • Excellent Chemical Resistance
  • Low Toxicity

SEPTON® grades are available with a range of Shore A hardness of 35-95 and tensile strengths of 290-5600 psi. SEPTON® resins are highly extendible with fillers, resins and oils, which allows formulation of a variety of hardness for adhesives, sealants and various compounds. As an additive, SEPTON® resins can be used to improve toughness of a variety of plastics. Several SEPTON® grades have U.S. FDA and USP Class VI approval.

SEPTON® has a versatile series of grades which can be used in numerous processing techniques such as blow molding, injection molding, extrusion, hot melt and solution coatings. SEPTON® resins are thermoplastics therefore, the scrap is recyclable without significant loss of properties.

When blended with a tackifier and a process oil, SEPTON® polymers provide hot melt adhesives having excellent heat and weather resistance.

SEPTON® Solubility:

  • Partial to Non-Soluble in: Ethyl Acetate, MEK, Methanol, Ethanol, Acetone, Water
  • Soluble in: Petroleum Ether, Toluene, Benzene, Hexane and Cyclohexane

Tackifiers Compatible with SEPTON®:

  • Rubber Phase: Acyclic Saturated Hydrocarbon resins, Hydrogenated Terpene resins, Petroleum resin and Hydrogenated Rosin resin
  • Styrene Phase: Aromatic resins and Styrenic resins

Formulation (parts by weight): SEPTON® 2063 - 100, Acyclic Saturated Hydrocarbon Resin - 250, Paraffinic Process Oil - 100

Information provided by The Kuraray Group.

Available Properties
  • Brookfield Viscosity
  • Peel Strength
  • Cohesion, Static Shear
  • Rolling Ball Tack Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。