Kuraray SEPTON® PM1, Polypropylene Modified Plastic
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic
Material Notes: Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block copolymers, which exhibit rubber-like properties over a wide range of temperatures. SEPTON®'s remarkable characteristics include:- Excellent Mechanical Properties
- Good Weatherability
- Excellent Low Temperature Properties
- Excellent Electrical Properties
- Superior Heat Resistance
- Excellent Chemical Resistance
- Low Toxicity
SEPTON® grades are available with a range of Shore A hardness of 35-95 and tensile strengths of 290-5600 psi. SEPTON® resins are highly extendible with fillers, resins and oils, which allows formulation of a variety of hardness for adhesives, sealants and various compounds. As an additive, SEPTON® resins can be used to improve toughness of a variety of plastics. Several SEPTON® grades have U.S. FDA and USP Class VI approval. SEPTON® has a versatile series of grades which can be used in numerous processing techniques such as blow molding, injection molding, extrusion, hot melt and solution coatings. SEPTON® resins are thermoplastics therefore, the scrap is recyclable without significant loss of properties. Formulation (parts by weight): PP (Block Copolymer) - 100, SEPTON® 2002 - 0 Information provided by The Kuraray Group.
| Available Properties |
- Melt Flow
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|