Kuraray HYBRAR® Low Rebound Compound # 2 Control
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® with ordinary styrenic soft compounds exhibit excellent rebound properties. Formulation (parts by weight): SEPTON® 4055 - 100, HYBRAR® 5127 - 0, Paraffin Oil - 180, Polypropylene - 50 Information provided by The Kuraray Group.
| Available Properties |
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Rebound
- Compression Set
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|