Multibase Multi-Flex® TPE A 5801 LC BLK
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer
Material Notes: Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and feature excellent heat and ozone resistance. LC products cover a wide temperature span from -40°F to 300°F. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
|
|
|
|