Multibase Multi-Flex® TPE A 8205 BLK
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer
Material Notes: Multi-Flex® A 8103 is an acoustic barrier compound that meets general motors specification GM2212M(FBMS 4-10). This specification is for a low flexural modulus product. The burn rate is 0.9 in/min (22.5 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Tear Strength
|
|
|
|