Multibase Multi-Flex® TPE A 8502 LC BLK
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer
Material Notes: Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and feature excellent heat and ozone resistance in addition to good low temperature performance. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
|
|
|
|