Multibase Multi-Flex® TPE A 8502 P BLK, 37.5% Filler Content
Subcategory: Elastomer, TPE; Thermoplastic; Polymer
Key Words: Thermoplastic Elastomer
Material Notes: The following data represents the actual data obtained from Lot # 941101-5. The moisture content is 0.03%. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tear Strength
|
|
|
|