Multibase Multi-Flex® TPE A 8620 BLK
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer
Material Notes: Formulated TPE compound is based on Shell's Kraton G resin and is widely used in automotive applications exhibiting a wide temperature range, replacing in many applications conventional thermoset rubber. Multibase is a licensed compounder for Shell's Kraton G polymers. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tear Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|