Multibase Multi-Flex® TPE A 8832 C BLK
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer
Material Notes: This product is based on Shell's Kraton G and is used for acoustic barrier applications, exhibiting high flexibility and ease of installation. It is made exclusively for Cascade Engineering. This product meets SD2-234 specifications, Harrison Radiator, CMP UP 01 AA, and GM 2217 M. The burn rate is 0.09 in/min (2.25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tear Strength
|
|
|
|