Multibase Multi-Flex® TPO 1047-4107
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Polyolefin
Material Notes: Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags. Data provided by Multibase.