Multibase Multi-Flex® TPO D-6206
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Polyolefin
Material Notes: This TPO product was developed for facia applications exhibiting adhesion for current automotive paint systems. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Gardner Impact
- Tear Strength
|
|
|
|