Multibase Multi-Flex® TPO D-6403
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Polyolefin
Material Notes: Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Tear Strength
|
|
|
|