Multibase Multi-Flex® TPO D-6509
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Polyolefin
Material Notes: Multi-Flex® A-6509 thermoplastic elastomer blend is designed to provide processors with cost effective compounds with excellent tear strength, tensile strength and high elongation. Multi-Flex® A-6509 features good injection molding and extrusion flow characteristics. Parison strength is excellent for blow molding applications. Pre-drying prior to processing is usually not necessary as with other thermoplastic elastomers. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Izod Impact, Notched
- Tear Strength
|
|
|
|
| Property Data |