Multibase Multi-Flex® TPO D-6601
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Polyolefin
Material Notes: Multi-Flex® D 6601 is filled TPO product with suitable UV stability for outdoor applications. Excellent impact properties, suitable flow characteristics for profile extrusion applications such as trail shields. Ash is 31.5% per ASTM D-955-89. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Tear Strength
|
|
|
|