Multibase Multi-Pro 2510 XGW High Gloss Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperature requirements. Product has UL approval. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Gardner Impact
- Flammability, UL94
- Gloss
|
|
|
|