Multibase Multi-Pro 2507 T NAT, 25% Filler Content Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: PP
Material Notes: Moisture is less than 0.06%. Multi-Pro 2507 T Natural is designed for high impact and high flexural strength. It can easily be colored and is FDA approved. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |