Multibase Multi-Pro 1012 C BLK Medium Impact, Mineral Filled Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: PP
Material Notes: Mineral filled PP compound for interior automotive applications. Product meets GMP PP 056 and EBG-M4 D605-A specifications. Ash is 10%. Data provided by Multibase.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
|
|
|
|