Multibase Multi-Pro 5012 C Natural, 50% Filler Content Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: PP
Material Notes: This product is well suited to fabricate non-glossy appliance parts, such as a vacuum cleaner canister. It replaces ABS at favorable cost performance characteristics. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Gardner Impact
|
|
|
|