Multibase Multi-Pro 2005 RC I High Impact, 20% Glass Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: PP
Material Notes: Multi-Pro 2005 RC I is a chemically coupled polypropylene compound with increased stiffness, flex strength and excellent impact resistance. This product is geared for top engineering plastics applications in the automotive industry. Data provided by Multibase.
Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|