Multibase Multi-ABS 3832 Natural
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than normal impacts, both notched izod and gardner, than typical High Heat ABS. Data provided by Multibase.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|