Asahi Kasei Tenac®-C 7554 Copolymer Acetal Resin
Subcategory: Acetal; Thermoplastic
Key Words: Tenac-C
Material Notes: High flow grade, with properties necessary for VCR reels Information provided by Asahi Kasei Corporation.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|