Asahi Kasei Tenac-C® LV450 Copolymer Polyacetal Resin
Subcategory: Acetal; Thermoplastic
Material Notes: Applications: Automotive: Gears, Slides, Switches, Guides Electrical and Industrial: Gears, Slides, Railings, CamsInformation provided by Asahi Kasei
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength, Yield
|
|
|
|
| Property Data |