Asahi Chemical Tenac® GT525 Acetal Homopolymer, 25% Glass Beads
Subcategory: Acetal; Thermoplastic; Polymer
Close Analogs: This product is not a part of the standard product line dated 2003.
Material Notes: 25% glass beads-filled grade with superior isotropic dimensional stability. Applications: Speedometer frames. Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Taber Abrasion, mg/1000 Cycles
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|