Kuraray Company Septon™ 2043 Thermoplastic Rubber

 

Subcategory: Elastomer, TPE; Thermoplastic

Close Analogs: Currently not a part of the current Kuraray product line.

Key Words: Thermoplastic Elastomer, TPE

Material Notes:
2043 is a Triblock (SEPS) copolymer. Septon™ is comprised of polystyrene blocks and soft polyolefin rubber blocks. It exhibits rubber-like properties over a wide range of temperature, although it flows like a thermoplastic at high temperatures. It has excellent elasticity and tensile strength without vulcanization, excellent heat aging resistance and low temp properties (Tg of rubber blocks is -53°C), affinity for olefinic and styrenics polymers, high electrical insulation, resistant to acids, alkalis, and alcohols, and low toxicity. Supplied in pellet form.

Applications:
Plastics modification: When blended with olefinic plastics, Septon™ improves physical properties such as impact strength and acts as a compatibilizer between olefinic and styrenic plastics.
Adhesives: When blended with tackifier and process oil, Septon™ affords adhesives having excellent heat resistance and weather resistance.

Information provided by LarSan Chemical Company.

Available Properties
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。