Kolon Kopa® N-66 KN333MT30 N-66 Nylon 66 Resin
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66; PA66; PA 66
Material Notes: KOPA is a thermoplastic resin with excellent mechanical, thermal and electrical properties. KOPA is widely used in the automobile, electrical and industrial parts. General KOPA N-66 features: High tensile strength, Outstanding self lubrication and abrasion resistance, Excellent chemical resistance, High usage temperature. Information provided by US distributor, API-Kolon.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Arc Resistance
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|