Lanxess Durethan® KL1-2218/40 H2.0 Nylon 66, Mineral/Glass Filled
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: PA 66, injection molding grade, 40% mineral/glass fiber, heat aging stabilized, Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|