Lanxess Durethan® KU2-2183 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: PA 6, injection molding grade, non-reinforced, good flowability, easy release, fast cycling, UL94 V-2 at 0.8 mm (in house test). , Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Tensile Modulus
- Comparative Tracking Index
- Melting Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |