Lanxess Pocan® B 3215 Z PBT, Glass Filled
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: PBT, injection molding grade, 10% glass fibers, elastomer modified, very good processability, good strength properties, Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Flammability, UL94
|
|
|
|