Lanxess Pocan® DP 2004 PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: PBT, injection molding grade, non-reinforced, UL 94V-2 from minimum thickness 0.75 mm (listed), max. temperature in glow wire test: 960 at 2 mm, "free of halogen", Electro Sector, Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|