Lanxess Pocan® DP 7043 PBT + ASA, Glass Filled
Subcategory: Polyester, TP; ASA Polymer; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: PBT/ASA-blend, injection molding grade with 30% glass fibers, low tendency to warp, good surface quality. , Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|