Lanxess Pocan® KU2-7503/1 Z PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: PBT, injection molding grade, non-reinforced, elastomer modified, UL94 V-0 at 0.8 mm ( all colors), non-migrating flame retardant additives., Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|