Lanxess Pocan® KU2-7604 PBT + PC
Subcategory: Polycarbonate; Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: PBT/PC blend, injection molding grade, non-reinforced, UL94 V-0 at 1 mm ( all colors), low tendency to warp., Property data per ISO test methods. Information provided by Lanxess.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Flammability, UL94
|
|
|
|