Techno Polymer Company Techno ABS LM100, Transparent
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Excellent shock resistance, rigidity, and processability. Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
- Processing Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |