LATI LATER 4E61 CERG/450-V0 45% Mineral and Glass Fiber Filled Polybutyleneterephthalate (PBT)
Subcategory: Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: Later thermoplastics are polybutyleneterephthalate (PBT) products. Later thermoplastic polyesters are suitable for injection molding, and are distinguished by good wear resistance, chemical inertness and low water absorption values. All Later versions can be used for products working in wet environments or in water. Because of its weak resistance to hydrolysis the use of the basic resin in continuous or protracted contact with hot water (higher than 50°C) is not advisable. Glass Reinforced Later grades feature low mold shrinkage with good mechanical properties; their rigidity increases substantially in versions with higher glass fiber contents. Later's with mineral fillers are recommended where no particular high impact resistance is necessary, but rigidity, high dimensional stability, and tight tolerances are required.Specific Notes for this Material: UL94 V-0 self-extinguishing, with halogens; 45% mineral fillers and glass fiber; high dimensional stability; good rigidity; low impact strength; excellent electric properties. Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Flexural Modulus
- Charpy Impact Unnotched
- Izod Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Heat Resistance - Ball Test (125°C)
- Heat Resistance - Ball Test (165°C)
- Injection Speed
- Needle Burner Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|