LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
Subcategory: Polyphenylene Ether/PPO; Thermoplastic; Polymer
Material Notes: Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most important properties featured by the Larils which can therefore be used within a wide range of temperatures (-40°C / +110°C). The Larils feature exceptional resistance to hydrolysis and are therefore applicable also in contact with very hot water. Specific Notes for this Material: UL94V-1 self extinguishing without halogens or red phosphorus; 30% glass fiber; excellent dimensional stability; low thermal linear expansion coefficient; high rigidity; good general mechanical properties; good creep resistance. Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Heat Resistance - Ball Test (125°C)
- Heat Resistance - Ball Test (165°C)
- Injection Speed
- Needle Burner Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|