LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
Subcategory: Polyurethane, TP; Thermoplastic; Polymer
Material Notes: Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These properties make the Lastanes very suitable for wheels, gears, couplings, parts of textile machinery, shoes, and others. Reinforced Lastanes are used when good rigidity and high dimensional stability are required.Specific Notes for this Material: 25% glass fiber; low molding shrinkage; good dimensional stability; high noise inertness; fair rigidity; good impact resistance even at low temperatures; good wear resistance. Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Dielectric Strength
- Comparative Tracking Index
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Heat Resistance - Ball Test (125°C)
- Heat Resistance - Ball Test (165°C)
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|