LATI LASTILAC 10 ABS/PC-Based Alloy
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Material Notes: Description: Lastilac products are ABS/PC-based alloys. Their excellent mechanical properties and thermal strength are clearly higher than those featured by ABS. These properties improve even more, starting from Lastilac 09 to reach their maximum values with Lastilac 11. The compounds are also distinguished by their dimensional stability and excellent surface finish. Excellent finishing allows for glossy colors and, if necessary, for metallized or chromed products. Specific Notes for this Material: good flowability; excellent gloss and surface finish; excellent impact strength; fair thermal strength. Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Dielectric Strength
- Comparative Tracking Index
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Heat Resistance - Ball Test (125°C)
- Heat Resistance - Ball Test (165°C)
- Injection Speed
- Needle Burner Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|