LATI LATISHIELD 90/13-07A-V1 Modified Polyphenylene Oxide (PPOm) Base E.M.I. Shielding Plastic (UL94 V-1)
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Material Notes: Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different types of granules, resulting in a homogeneous distribution of the shielding fiber reinforcement throughout the polymer mass during molding. No particular limitations exist on the basic product: filled, reinforced, self-extinguishing, and other materials can be used, except that great care should be given to handling and processing the granule, while steel fiber appearing on the surface of items produced in bright colors should be taken into account. The Latishields are used for molding business machine housings, containers for electronic devices (radio, telecommunications, defense and aeronautical systems, measuring equipment, electronic units for cars). In addition to the shielding effect, the Latishield s also feature good antistatic properties as well low resistivity which make them partially conductive.Specific Notes for this Material: modified polyphenylene oxide base (PPOm); UL94V-1 self-extinguishing; without halogens or red phosphorus. Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Flexural Modulus
- Izod Impact, Notched
- Surface Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|