LATI LARAMID G/50 50% Glass Filled Polyphtalamide (PPA) Based Compound
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: Description: Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphtalamide) offering improved performance compared to traditional engineering thermoplastics (such as polycarbonate, Nylons, polyesters and acetals) at a lower cost than specialty polymers (PEEK™ and liquid crystal polymers). Laramid offers excellent mechanical properties (strength, stiffness, fatigue and creep resistance) over a broad temperature range, exceptional thermal resistance good dimensional stability and good processing characteristics. Furthermore, it's properties are not affected much by typical moisture levels therefore Laramid compounds do not require critical drying procedures and can be easily employed for complicated part production using conventional molding equipment. Glass fiber reinforced Laramid requires accurate design to reduce differential shrinkage and to minimize warpage of parts.Specific Notes for this Material: PPA, 50% glass fiber Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsability arising from an improper use of the products described in this document. All data provided by LATI.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Flexural Modulus
- Izod Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|