LG Chemical RS-656 ABS Resin
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: This material is no longer in LG Chemical's product line
Key Words: Poly(Acrylonitrile Butadiene Styrene); LG Chemical Styrenics
Material Notes: Chemical resistance and high impact, Non-toxicity, Uniform sheet thickness in process of vacuum molding, Crack resistance, Good strength at low temperature and high temperature as well, Applications include liners for refrigerator doors and interiors Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- IEC 707 Flammability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|