LG Chemical 82TR SAN Resin
Subcategory: SAN Polymer; Thermoplastic
Key Words: Poly(Styrene Acrylonitrile); LG Chemical Styrenics
Material Notes: High clarity, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include window for VTR tapes, and dust covers for audio Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- IEC 707 Flammability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|