NILIT Polynil® P50FI Internally Lubricated Nylon 66
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long, thin flow lengths, like cable ties, connectors or industrial components.Key characteristics: - Excellent flow
- High elongation
- Good mould release
- High toughness
- Good thermal performance
- UL 94 V2 listed at 0.75 mm
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Loss On Ignition
- Viscosity Measurement
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched (ISO)
- Dielectric Strength
- Comparative Tracking Index
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Heat Resistance - Ball Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|