NILIT Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retardancy. Typical applications include high loaded circuit breaker components, isolator blocks and housings.Key characteristics: - Flame retardant
- Extremely high mechanical performance
- High CTI
- Low phosphate release
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Clamping Force
- Flammability Rating
- Heat Resistance - Ball Test
- Holding Pressure
- Needle Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|