NILIT Nilamid B3 H XB Unfilled, Impact Resistant PA6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include automotive components and industrial components subjected to shock loads.Key characteristics: - Good impact strength
- High elongation
- Good overall mechanical performance
- Excellent surface finish
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Vicat Softening Point
- Flammability, UL94
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Clamping Force
- Heat Resistance - Ball Test
- Holding Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|