NILIT Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its excellent processing characteristics it is often used in complicated components. Typical applications include electrical cooling fans and housings, fuse boxes and carriers, flame retardant cable ties and corrugated tube. This product can be supplied in a full range of colors and has an excellent surface finish. For this reason it is often used in aesthetical components, like public bathroom accessories or trash cans.Key characteristics: - Easy processing
- Good heat aging characteristics: UL RTI listing (mechanical) up to 140°C
- V0 listing at 0.75 mm
- Halogen and red phosphorous free
- Excellent CTI value (600 V)
- Good impact strength
- Good elongation
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Clamping Force
- Flammability Rating
- Heat Resistance - Ball Test
- Holding Pressure
- Needle Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|